Compared to Portland cements, calcium sulphoaluminate (CSA) cements are energy saving and low-CO2 hydraulic binders, due to the decrease of synthesis temperature and kiln thermal input associated with the reduced limestone requirement and carbon dioxide generation. Further enhancements in terms of environmentally friendly features can be achieved if some industrial wastes are used as partial or total substitutes for the natural materials (limestone, bauxite, gypsum) involved in the CSA cement manufacture. This paper deals with a laboratory investigation of synthetic CSA clinkers generated in an electric oven at 1150°, 1200°, 1250° and 1300°C from raw mixtures containing (i) bottom ash derived from the fluidized bed combustion (FBC) of coal (essentially a source of noncarbonated lime and calcium sulphate) and (ii) anodization mud (AM) or alumina powder (AP), Al2O3 rich by-products originated by the production of anodized aluminium elements and the secondary aluminium manufacture, respectively. Six bauxite-free ternary blends, containing 10-35% limestone plus 0-31% natural gypsum or 0-40% FBC bottom ash plus 0-69% AM or 0-50% AP, and four binary blends, consisting only of 37-60% FBC bottom ash and 52-63% AM or 40-45% AP, were explored. They were generally more suitable than a reference mixture composed by 42% bauxite, 33% gypsum and 25% limestone. XRD analysis showed a complete conversion of reactants and a very good selectivity towards C A S 4 3 , the main CSA cement component.

Low-carbon calcium sulphoaluminate cements synthesized from industrial wastes and by-products

TELESCA, ANTONIO;MARROCCOLI, Milena;PACE, MARIA LUCIA;VALENTI, Gian Lorenzo
2012-01-01

Abstract

Compared to Portland cements, calcium sulphoaluminate (CSA) cements are energy saving and low-CO2 hydraulic binders, due to the decrease of synthesis temperature and kiln thermal input associated with the reduced limestone requirement and carbon dioxide generation. Further enhancements in terms of environmentally friendly features can be achieved if some industrial wastes are used as partial or total substitutes for the natural materials (limestone, bauxite, gypsum) involved in the CSA cement manufacture. This paper deals with a laboratory investigation of synthetic CSA clinkers generated in an electric oven at 1150°, 1200°, 1250° and 1300°C from raw mixtures containing (i) bottom ash derived from the fluidized bed combustion (FBC) of coal (essentially a source of noncarbonated lime and calcium sulphate) and (ii) anodization mud (AM) or alumina powder (AP), Al2O3 rich by-products originated by the production of anodized aluminium elements and the secondary aluminium manufacture, respectively. Six bauxite-free ternary blends, containing 10-35% limestone plus 0-31% natural gypsum or 0-40% FBC bottom ash plus 0-69% AM or 0-50% AP, and four binary blends, consisting only of 37-60% FBC bottom ash and 52-63% AM or 40-45% AP, were explored. They were generally more suitable than a reference mixture composed by 42% bauxite, 33% gypsum and 25% limestone. XRD analysis showed a complete conversion of reactants and a very good selectivity towards C A S 4 3 , the main CSA cement component.
File in questo prodotto:
File Dimensione Formato  
Paper 102_Telesca et alii.pdf

non disponibili

Tipologia: Documento in Post-print
Licenza: DRM non definito
Dimensione 227.36 kB
Formato Adobe PDF
227.36 kB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11563/35868
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact